Skripsi
OPTIMASI FORMULA HYDROGEL SCAFFOLD DENGAN NANOPARTIKEL BESI OKSIDA GAMBIR DAN EPIGALOKATEKIN GALAT TEH HIJAU SEBAGAI CROSSLINKER UNTUK AGEN HEMOSTASIS
Bleeding is a medical condition that requires rapid and effective management because it can lead to severe complications and death. The development of hydrogel scaffolds has emerged as a promising hemostatic approach due to their threedimensional porous structure, fluid absorption capacity, and ability to support blood clot formation. Iron oxide nanoparticles (IONP) enhance hemostatic activity by promoting blood clot formation, while epigallocatechin gallate (EGCG) serves as a natural cross-linker to improve hydrogel scaffold performance. This study aimed to optimize a hydrogel scaffold formulation using two main polymers, alginate and konjac glucomannan (KGM), and different concentrations of green tea-derived EGCG as a cross-linker, with the addition of gambir-based iron oxide nanoparticles synthesized through a green synthesis approach for hemostatic application. The gambir extract functions as a reducing and stabilizing agent in the nanoparticle synthesis process. The study involved extract preparation and standardization, phytochemical screening, determination of total phenolic content, synthesis of iron oxide nanoparticles, hydrogel scaffold formulation, and optimization using a 2² factorial design. The optimization responses included porosity, blood clotting index (BCI), centrifuge retention capacity (CRC), and moisture content (MC), followed by characterization of the optimum formula using FTIR, SEM, BET, and XRD. The results showed that the total phenolic content of green tea extract was 328.666 ± 53.266 mg GAE/g and that of gambir extract was 230.844 ± 1.150 mg GAE/g, while XRF analysis revealed an Fe content of 68.149 ± 0.034% in the synthesized iron oxide nanoparticles. The optimum formula was obtained using KGM and 0.5% EGCG, with a desirability value of 0.944, yielding porosity of 399.916%, BCI of 32.479%, CRC of 327.555%, and MC of 16.723%. Characterization of the optimum formula demonstrated intermolecular functional group interactions, a porous surface morphology with blood cell adhesion, a specific surface area of 62.008 m²/g, and a crystallite size of 3.915 Å. In conclusion, the KGM-based hydrogel scaffold containing 0.5% EGCG and gambir-derived iron oxide nanoparticles has potential to be developed as a hemostatic agent.
No other version available