Skripsi
ANALISIS MIKROSTRUKTUR MORTAR DENGAN PENAMBAHAN NANOSILIKA HASIL SINTESIS HIDROTERMAL DARI FLY ASH
Portland cement-based mortar possesses a relatively porous microstructure, which may adversely affect its strength and durability. This study aimed to investigate the effect of hydrothermally synthesized fly ash-derived nanosilica on the microstructure and compressive strength of mortar. Nanosilica was synthesized from fly ash using a hydrothermal method. Mortar mixtures were prepared with nanosilica contents of 0%, 3%, 6%, 9%, and 12% by weight of cement. Compressive strength tests were conducted at 28 days, while microstructural characterization was performed using X-Ray Diffraction (XRD) and Scanning Electron Microscopy (SEM). The results showed that the incorporation of nanosilica influenced both the compressive strength and microstructure of mortar. The compressive strength increased from 13.04 MPa for the control mortar to 17.95 MPa at 3% nanosilica and reached a maximum value of 24.21 MPa at 12% nanosilica. However, a reduction in compressive strength to 13.85 MPa was observed at the 6% nanosilica content. XRD analysis revealed an increase in the amorphous phase content from 74.54% to 80.13%. SEM observations showed microstructural differences among the mixtures, with the densest and most homogeneous microstructure observed at 12% nanosilica. The improvement in compressive strength was attributed to the increased amorphous phase content and microstructural densification resulting from the pozzolanic reaction of nanosilica, whereas the strength reduction at 6% was likely associated with particle agglomeration. Hydrothermally synthesized fly ash-derived nanosilica improved the microstructure and compressive strength of mortar, with optimum performance achieved at a nanosilica content of 12%.