The use of lightweight concrete is commonly found in structures to minimize the total dead load of Glass powder on the microstructure and compressive strength properties of concrete, focusing on X-Ray Diffraction (XRD) and Scanning Electron Microscope (SEM) testing after curing for 28 days. In this study, test samples were taken from concrete fragments that had been tested for specific gravity …