The production of rubber leaf biobriquettes has been carried out with variations in carbonization time and variations in the concentration of dammar resin adhesive, characterized based on the SNI 01-6235-2000 standard. Rubber leaves were carbonized using a pyrolysis reactor for 60, 90, and 120 minutes at a temperature range of 400°C-500°C. The charcoal from the rubber leaves was ground, then …